Cold-Heading Titanium Wire for Fasteners

Cold-Heading Titanium Wire for Fasteners

Heavy-Coil Titanium Wire for Continuous Fastener Cold Heading

Cold heading turns wire into fastener blanks in one continuous stroke sequence, at a rate that machining from bar cannot approach. With titanium the limiting factor is often the wire itself: small coils mean frequent stops to re-thread the header, and uncoated wire tends to gall against carbide dies.

Through a qualified partner mill, we supply Ti-6Al-4V heavy-coil wire of above 150 kg and up to 200 kg per coil, coated with a dry-film lubricant so it can feed a header continuously.


Technical Data (Partner-Mill Figures)

PropertyValueNote
Diameter rangeΦ2.0–8.0 mm
Diameter tolerance−0.02 / 0 mmTight limit for header feed
Coil weightabove 150 kg, up to 200 kgHeavy coil for continuous heading
Hydrogen / oxygenH ≤ 0.0125%, O ≤ 0.20%Based on GB/T 3620.1
Al / V uniformity≤ 0.25% variation within an ingot, ≤ 0.35% between ingotsConsistent heading behaviour from coil to coil
MicrostructureTransverse A1–A3, longitudinal AA1–AA3Rated to the mill’s microstructure charts
Annealed conditionRm 900–1150 MPa, A > 12%
Solution treated & agedRm > 1138 MPa, Rp0.2 > 1069 MPa, A > 10%, Z > 20%
Shear strength (STA)> 670 MPa
Lubricant coatingDry film, 3–10 µmUniform thickness for continuous upsetting

Guaranteed values for your order — including any cold-upset test, surface inspection (e.g. eddy current) and microstructure rating — are written into the purchase order and reported on the MTC.


Why Heavy Coils and Dry-Film Coating Matter

  • Fewer line stops: a 150–200 kg coil keeps a header running far longer between coil changes than small coils do.
  • Less die galling: titanium tends to cold-weld to carbide tooling; an even 3–10 µm dry-film coating keeps lubrication consistent through each stroke.
  • Controlled hydrogen: hydrogen is limited to H ≤ 0.0125% to reduce the risk of hydrogen embrittlement in finished fasteners.
  • Consistent chemistry: tight Al and V uniformity within and between ingots means heading parameters set on one coil carry over to the next.

Quality Documents

Each coil is supplied with a material test certificate showing heat chemistry and mechanical test results. Additional tests and acceptance criteria are agreed per order.

Request a Quote for This Product

Send your drawing or specification and we will reply within 24 hours.

Get a Quote
Quick Contact

Reply within 24 hours 🔒 NDA available on request — your drawings stay confidential 📦 Small quantities ship as LCL; larger orders ship as full containers for simpler loading and customs inspection.

WhatsApp
Quality Assurance
  • ✓ Material Test Certificate (MTC) with Every Order
  • ✓ ASTM / ASME / AMS Standard Compliance
  • ✓ Third-party Inspection Available
Request MTC / Test Report
Related Products

Ready to Start Your Project?

Send your drawing or specification and we will reply within 24 hours.

Get a Quote
Quick Inquiry
WhatsApp