Type something to search...

Titanium Water Jet Cutting

Titanium Water Jet Cutting

Titanium Water Jet Cutting

Every thermal cutting route leaves something behind in titanium. Laser and plasma leave a heat affected zone and heat tint. Above roughly 500 °C in air, titanium also picks up oxygen and forms alpha case — a hard, brittle surface layer that cracks in forming and welding, dulls carbide end mills, and is invisible on the surface.

Abrasive water jet cutting through our certified partner facilities leaves none of it. The cutting temperature at the workpiece stays near ambient. There is no heat affected zone, no alpha case, and no discoloration to pickle off afterwards.

For anything that gets finish-milled, formed, welded or fatigue-loaded after cutting, that is the whole argument.

What You Are Actually Buying

No post-cut pickling on the edge. A laser or plasma cut edge on titanium usually needs pickling and alpha case removal before the part moves on. A water jet edge does not. On a part with a long cut perimeter, that removed operation is often the real cost difference — not the cutting rate.

No mechanical property change at the edge. The material at the cut face has the same properties as the material 10 mm (0.394”) away. For fatigue-critical parts, CNC machine shop preforms, and anything going into a welded joint, this matters more than surface finish.

Thickness reach. Abrasive water jet cuts titanium well past the practical limit of laser on this material. Thick plate that no laser will take cleanly is routine on a water jet — slowly, but cleanly.

Near-Net-Shape Blanks for Machine Shops & Knife Makers

Combining cold abrasive water jet profiling with Surface-Ground & 6-Side Milled Blanks through our partner network eliminates the two biggest bottlenecks in titanium secondary machining: surface scale distortion and slow perimeter roughing.

  • For Knife Making & Custom EDC Studios: Starting with double-side surface-ground Grade 5 (Ti-6Al-4V / UNS R56400 / Werkstoff 3.7165 / ВТ6) sheet in 1.0–5.0 mm (0.040"–0.197") thickness, cold water jet cuts knife scale and frame-lock blanks directly to near-net perimeter with undersized pivot and screw holes ready for reaming or CNC finishing. Because there is zero heat-affected zone and no brittle alpha case on the cut edge, micro-carbide end mills and chamfer tools do not chip on entry. Parts can also be nested strictly along the specified Rolling Grain Direction so every frame-lock spring bar exhibits uniform lockbar tension.
  • For CNC Machine Shops & Subsea Fabricators: On medium and heavy plate from 6.35–76.2 mm (0.250"–3.000") in Grade 2 (UNS R50400 / Werkstoff 3.7035 / ВТ1-0), Grade 5 (UNS R56400 / Werkstoff 3.7165 / ВТ6), and Grade 23 ELI (UNS R56407 / Werkstoff 3.7165-ELI / ВТ6С), water jet cutting produces near-net-shape contour preforms for marine and subsea housings, manifolds, and structural brackets — dramatically reducing 3-axis and 5-axis hogging time, chip volume, and spindle load.

What It Costs You

Kerf taper. The jet loses energy as it passes through the material, so the kerf is slightly wider at the top than the bottom. On thin sheet this is negligible. On thick plate it is not, and it has to be either accepted, compensated by a tilting head, or machined out. If your part has a tight profile tolerance through the full thickness, say so at quotation — tolerances and cutting allowances are confirmed per drawing and order specification.

Speed. Water jet is slower than laser on thin material, sometimes by a large factor. On sheet under about 3 mm (0.118”) where alpha case is not a concern for the application, laser is usually the better commercial answer.

Garnet embedding. The abrasive is a mineral, and a small amount embeds in the cut edge. For structural parts or blanks that will be finish-milled around the perimeter this is irrelevant. For medical instruments, semiconductor and high-purity chemical service, the edge needs cleaning or light machining afterwards. Flag the application and it gets handled — it is not a defect, but it is not automatically acceptable either.

Edge finish varies with speed. Cut quality is a commercial choice, not a fixed property: a slow pass gives a smooth, near-uniform edge; a fast separation pass leaves visible striation toward the bottom of the cut. Specify which you need rather than assuming the finest.

Choosing Between Routes

Water jetLaserBand saw
Heat affected zoneNoneYesNone
Alpha case riskNoneYes, needs picklingNone
Thin sheet economicsPoorBestNot possible
Thick sectionGoodLimitedStraight cuts only
ContoursYesYesNo

See cut to length for the full comparison.

Ordering & Documentation

Send the drawing or DXF, the grade and thickness, the quantity, the profile tolerance you need through the thickness, any rolling grain direction requirement, and what happens to the part next. Every shipment is supplied with a Material Test Certificate (MTC) with heat-lot traceability and Certificate of Conformance (CofC).

Request a Water Jet Cutting Quote →

Frequently Asked Questions

When is water jet the right choice for titanium instead of laser?
When the part cannot tolerate heat input: thick plate, fatigue-critical parts, and anything formed, finish-milled, or welded after cutting. Water jet cuts cold, so there is no heat-affected zone, no alpha case and no discoloration. On thin sheet under about 3 mm (0.118"), laser is usually the better commercial answer.
Does water jet cutting change the material properties at the edge?
No. The material at the cut face has the same properties as the base material, which is the main reason to choose water jet for fatigue-critical parts, CNC roughing preforms, and weld preparations.
What files do you need for a water jet cutting quote?
DXF or DWG for flat profiles; STEP, IGES or PDF drawings also work. Attach them to the inquiry form (up to 25 MB) together with grade, thickness and quantity. Tolerances and lead times are confirmed per drawing and order specification.
Can abrasive from the jet stay in the cut edge?
A small amount of garnet embeds in any abrasive water jet edge. For structural parts and blanks that undergo subsequent perimeter milling it is irrelevant; for medical, semiconductor or high-purity chemical service the edge is cleaned or lightly machined afterwards — flag the application at quotation.