Grade 2 (CP Titanium) vs Grade 5 (Ti-6Al-4V) — Complete Comparison

Grade 2 (UNS R50400) is unalloyed commercially pure alpha titanium engineered for cold formability, multi-pass weldability, and chemical corrosion resistance (345+ MPa tensile), while Grade 5 (Ti-6Al-4V, UNS R56400) is an alpha-beta alloy delivering 895+ MPa tensile strength for high-load structures.

Property Grade 2 (CP Titanium) Grade 5 (Ti-6Al-4V)
Metallurgical Type Commercially Pure (α) α+β Alloy (6% Al, 4% V)
Density (g/cm³) 4.51 4.43 ★
Tensile Strength (MPa) 345-450 895-1000 ★
Yield Strength (MPa) 275-410 828-910 ★
Elongation (%) 20-28 ★ 10-15
Weldability & Cold Forming Excellent ★ Moderate (requires strict shielding)
FOB China main port cost benchmark (USD/kg) $14-24 ★ $22-38
Seawater Corrosion Resistance Immune (<80°C) Immune (<80°C)

Choose Grade 2 (CP Titanium) When

  • ✓ Shell-and-tube heat exchangers (ASTM B338)
  • ✓ Chemical reactors, tanks, and process piping
  • ✓ Cold bending, stamping, or extensive field TIG welding
  • ✓ Corrosion service where 275 MPa yield strength is sufficient

Choose Grade 5 (Ti-6Al-4V) When

  • ✓ Aerospace airframe brackets, shafts, and fasteners
  • ✓ High strength-to-weight CNC machined components
  • ✓ High-pressure subsea and motorsport hardware
  • ✓ Dynamic fatigue loading applications

Engineering Trade-Off Analysis: Grade 2 (CP Titanium) vs. Grade 5 (Ti-6Al-4V)

Mechanical Strength vs. Cold Formability: Grade 2 has a minimum yield strength of 275 MPa and 20% minimum elongation, allowing tight-radius tube bending, plate rolling, and hydroforming without cracking. Grade 5 triples the yield strength (828+ MPa) through 6% Al and 4% V alloying, but requires hot forming or precision CNC machining.

Weldability in Process Equipment: Grade 2 can be TIG/GTAW welded in the field using ERTi-2 filler wire with ductile, corrosion-matched weldments—making it the global workhorse for ASTM B338 heat exchangers and reactors. Grade 5 is weldable with ERTi-5 filler but requires stricter inert gas trailing shield protection and post-weld stress relief.

Corrosion Parity & Cost Difference: In seawater, neutral chlorides, and oxidizing acids up to 80°C, Grade 2 and Grade 5 exhibit virtually identical oxide-film corrosion immunity. If high structural strength is not required, specifying Grade 2 saves 30%–45% in material and fabrication cost.

Not sure which material is right for your project?

Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.

Related Comparisons

Ready to Start Your Project?

Send your drawing or specification and we will reply within 24 hours.

Get a Quote
Quick Inquiry
WhatsApp