Grade 5 (Ti-6Al-4V) vs Grade 23 (Ti-6Al-4V ELI) — Complete Comparison

Grade 23 (Ti-6Al-4V ELI — Extra Low Interstitials, UNS R56401) is the higher-purity variant of Grade 5 (UNS R56400), restricting maximum oxygen to 0.13 wt% (vs. 0.20 wt% in Grade 5) and iron to 0.25 wt% to maximize fracture toughness, crack-growth resistance, and medical biocompatibility.

Property Grade 5 (Ti-6Al-4V) Grade 23 (Ti-6Al-4V ELI)
UNS Designation R56400 (Ti-6Al-4V) R56401 (Ti-6Al-4V ELI)
Oxygen Max (wt%) 0.20 0.13 ★
Iron Max (wt%) 0.30-0.40 0.25 ★
Tensile Strength (Min) (MPa) 895 ★ 828-860
Yield Strength (Min) (MPa) 828 ★ 759-795
Fracture Toughness (K_Ic) Good (~55-75 MPa√m) Superior (~75-100 MPa√m) ★
Implant Certification ASTM F1472 (instruments/non-ELI) ASTM F136 / ISO 5832-3 ★
Cost Difference Standard baseline ★ +10-15% Triple-VAR ELI premium

Choose Grade 5 (Ti-6Al-4V) When

  • ✓ Aerospace airframe structures (AMS 4928)
  • ✓ Industrial, automotive, and marine high-strength parts
  • ✓ Non-implanted surgical instruments and trays
  • ✓ Maximum static yield strength (828+ MPa) at lower cost

Choose Grade 23 (Ti-6Al-4V ELI) When

  • ✓ Orthopedic, spinal, trauma, and dental implants (ASTM F136)
  • ✓ Fracture-critical aerospace damage-tolerant fittings (AMS 4930)
  • ✓ Cryogenic service (-196°C to -253°C)
  • ✓ Thin-wall bionic actuator shafts requiring impact toughness

Engineering Trade-Off Analysis: Grade 5 (Ti-6Al-4V) vs. Grade 23 (Ti-6Al-4V ELI)

Interstitial Oxygen Control & Fracture Toughness: Lowering interstitial oxygen (O <= 0.13%), nitrogen (N <= 0.03%), and carbon (C <= 0.08%) slightly reduces minimum tensile strength (828–860 MPa for Grade 23 vs. 895 MPa for Grade 5), but significantly increases plane-strain fracture toughness (K_Ic) and fatigue crack propagation resistance.

Surgical Implant vs. Structural Standards: Grade 23 certified to ASTM F136 / ISO 5832-3 is the mandatory global standard for permanent orthopedic implants (spinal rods, hip stems, bone plates, dental abutments). Standard Grade 5 per ASTM B348 / AMS 4928 is used for airframe structures, surgical instruments, and industrial hardware.

Cryogenic Ductility Down to -253°C: Interstitial impurities cause embrittlement at liquid nitrogen (-196°C) and liquid hydrogen (-253°C) temperatures. Grade 23 ELI retains ductility and impact toughness at cryogenic temperatures, making it essential for space launch propellant tanks and cryogenic valves.

Not sure which material is right for your project?

Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.