Titanium (Grade 5) vs Inconel 625 — Complete Comparison
Titanium Grade 5 (Ti-6Al-4V) and Inconel 625 share comparable room-temperature tensile strength (~900 MPa), but Titanium weighs 47.5% less (4.43 g/cm³ vs. 8.44 g/cm³) and costs substantially less per unit volume, whereas Inconel 625 dominates extreme temperatures above 400°C.
| Property | Titanium (Grade 5) | Inconel 625 |
|---|---|---|
| Density (g/cm³) | 4.43 ★ | 8.44 |
| Tensile Strength (MPa) | 895-1000 | 827-1034 |
| Max Service Temp (°C) | 400 | 980 ★ |
| Corrosion Resistance | Excellent (seawater, oxidizing) | Excellent (reducing + oxidizing) ★ |
| Cost per kg (USD/kg) | $22-38 ★ | $80-150 |
| Part Weight (Equal Volume) | 47.5% lighter ★ | Baseline (1.9x heavier) |
Choose Titanium (Grade 5) When
- ✓ Weight reduction is critical (subsea risers, aerospace)
- ✓ Seawater, brine, and oxidizing chloride media
- ✓ Operating temperature is below 400°C
- ✓ Reducing per-part raw material cost vs. nickel alloys
Choose Inconel 625 When
- ✓ Continuous operating temperature exceeds 400–980°C
- ✓ Strong uninhibited reducing acids
- ✓ Extreme thermal creep and oxidation service
- ✓ Nuclear core or hot turbine exhaust components
Engineering Trade-Off Analysis: Titanium (Grade 5) vs. Inconel 625
Temperature Boundary (400°C Rule): Below 350–400°C, Titanium Grade 5 (and Grade 2/7/12 for chemical equipment) provides unmatched specific strength and chloride immunity at nearly half the weight of nickel superalloys. Above 450°C in air, titanium absorbs oxygen and nitrogen, so Inconel 625 or 718 must be used for hot gas turbines and exhaust manifolds.
Oxidizing Chlorides vs. Reducing Acids: In seawater, subsea risers, and wet chloride scrubbers, titanium matches or outperforms Inconel 625 at a fraction of the component weight. In concentrated reducing acids (such as hot uninhibited HCl or H2SO4), nickel-chromium-molybdenum alloys like Inconel 625 or Hastelloy C-276 are preferred.
Per-Part Volume Cost Advantage: Because Inconel 625 has nearly double the density of titanium (8.44 vs. 4.43 g/cm³), a machined titanium flange or subsea stress joint can need considerably less raw material by weight than the same part in Inconel 625.
Related Specifications, Grades & Mill Products
Not sure which material is right for your project?
Our engineers can recommend the optimal grade based on your specific application, environment, and budget requirements.